NYLON's toughness, low coefficient of friction and good abrasion resistance make it an ideal replacement for a wide variety of materials from metal to rubber. It weighs on 1/7 as much as bronze. Using nylon reduces lubrication requirements, eliminates galling, corrosion and pilferage problems, and improves wear resistance and sound dampening characteristics. NYLON has a proven record of outstanding service in a multitude of parts for such diverse fields as paper, textiles, electronics,more
Unit of Measure
Items
Nylon PA6MD

Nylon 6/6 MDS Sheet

Nylon PA6MD

Nylon 6/6 MDS Sheet

Nylon PA6MD

Nylon 6/6 MDS Sheet

Nylon PA6MD

Nylon 6/6 MDS Sheet

Nylon PA6MD

Nylon 6/6 MDS Sheet
Material N/A PA66+MoS2
Color N/A Gray MD
Thickness N/A 0.312 in N/A 0.375 in N/A 0.500 in N/A 0.625 in N/A 0.750 in
Sheet Size N/A 24 x 48 in
Optional Sheet Size N/A 12 x 48
Weight N/A 2.31 lb/ft² N/A 2.78 lb/ft² N/A 3.70 lb/ft² N/A 4.63 lb/ft² N/A 5.56 lb/ft²
Specific Gravity (ASTM D792) N/A 1.14
Density (ASTM D792) N/A 0.0412 lb/in³
Hardness - Rockwell (ASTM D785) N/A R121/M80
Water Absorption - Saturation (ASTM D570) N/A 8.5 %
Tensile Strength - Ultimate (ASTM D638) N/A 12400 psi
Tensile Modulus (ASTM D638) N/A 470000 psi
Elongation at Break (ASTM D638) N/A 90 %
Flexural Strength at Yield (482ºF/250ºC) N/A 17000 psi
Flexural Modulus N/A 410000 psi
Impact Strength, Notched at 73°F (ASTM D256) N/A 1.2 ft·lb/in
Dynamic Coefficient of Friction at 40 psi, 50 fpm N/A 0.28
Coefficient of Linear Thermal Expansion N/A 4 x 10-5 in/in/ºF
Heat Deflection Temperature at 66 psi N/A 465 ºF
Heat Deflection Temperature at 264 psi N/A 194 ºF
Maximum Operating Temp. - Short Term N/A 355 ºF
Maximum Operating Temp. - Long Term N/A 185 ºF
Dielectric Strength (ASTM D149) N/A 350 V/m
Volume Resistivity (ASTM D257) N/A 1015 ohm·cm
Flammability at .118" UL94 N/A V2
Availability N/A stock